DIN17175 Grade 16Mo3 Steel Tube
Specification
- Standards: DIN 17175, EN 10028
- Size: OD:10.2-711mm; WT:1.6-100mm; L:5.8m,6m,11.8m or random.
- Technical: Normalizing, Quenching and Tempering, Normalizing and Tempering.
- Application: Used in the power plant boiler tubes, etc
Material 16Mo3 is non-alloy steel with high-temperature properties, good plasticity, toughness, cold bending and welding properties according to German and European standards DIN EN17175 and DIN EN 10028, is mainly used the manufacture of pressure vessels, boilers and heat exchangers and steam pipes.
16mo3 steel pipe equivalent
Germany | France) | UK | GB |
DIN 1715515Mo3 | NFA 36–205 –15D3 | BS1501–243b | 12Cr1MoV |
16Mo3 Chemical Composition
C | Si | Mn | P | S | Cr | Mo |
0.12-0.2 | ≤0.35 | 0.4-0.9 | ≤0.025 | ≤0.020 | 0.3 | ≤0.35 |
16Mo3 Mechanical Property
Grade | Tensile strength Rm | Yield strength YS | Enlongation A(%) |
16Mo3 | 450-600 | 280 MPa | 22 |
16Mo3 Pipe Outside Diameter & Tolerance
Hot rolled
|
Outside Diameter, mm
|
Tolerance
|
OD≤219.1
|
±1% or ±0.5mm
|
|
OD>219.1
|
±1% or ±0.5mm
|
|
Cold Drawn
|
Outside Diameter, mm
|
Tolerance
|
OD≤114
|
±0.5% or ±0.3mm
|
16Mo3 Pipe Wall thickness & Tolerance
Hot rolled
|
Outside Diameter, mm
|
WT/OD
|
Tolerance
|
OD≤219.1
|
WT/OD≤2.5%
|
±12.5% or ±0.4mm
|
|
2.5%<WT/OD≤5%
|
|||
5%<WT/OD≤10%
|
|||
WT/OD>10%
|
|||
OD>219.1
|
WT/OD≤2.5%
|
±20%
|
|
2.5%<WT/OD≤5%
|
±15%
|
||
5%<WT/OD≤10%
|
±12.5%
|
||
WT/OD>10%
|
±10%
|
||
Cold Drawn
|
Outside Diameter, mm
|
–
|
Tolerance
|
OD≤114
|
–
|
±10% or ±0.2mm
|
Material 16Mo3 is the commonly used alloy grade specified in EN 10028 and EN17175 standard. WLD steel supply and stock the 16Mo3 seamless steel pipe in various sizes and specifications, delivered by heat treatment normalized or normalizing + tempering, which is a common material in the boiler system. WLD steel not only do we have all kinds of sizes and other material, but we also have all kinds of sizes that are hard to find.